Hi!
Use copper sulphate soln only as it reacts with CS gives pink indication on cs surface which ensures contamination free surface
Regards
Hegde


On Sun, 1 Jul 2018 at 11:06, Ankit Gandhi
<asgandhi.90@gmail.com> wrote:
Dear sir,
Will you tell me technique to identify cut back area.
As we are doing CuSO4 for SS clad plate is there any similar method available for cupronickel clad plate to identify clad removal of cu.

Regards,
Ankit Gandhi

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...