[MW:28014] Re: Welding of CuNi 70/30 to SA106

Dear sir,
Will you tell me technique to identify cut back area.
As we are doing CuSO4 for SS clad plate is there any similar method available for cupronickel clad plate to identify clad removal of cu.

Regards,