Sunday, July 1, 2018

[MW:28014] Re: Welding of CuNi 70/30 to SA106

Dear sir,
Will you tell me technique to identify cut back area.
As we are doing CuSO4 for SS clad plate is there any similar method available for cupronickel clad plate to identify clad removal of cu.

Regards,
Ankit Gandhi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs