Re: [MW:26776] VALIDATION OF THE WELDING PROCESS FOR THE HARD FACING AND SEAT RING OF THE GATE VALVES

Hi ,

Its good to see your mail subject regarding validation , There is separate clause in API SPEC Q1 & API 5LD Section 7.5.2

Here are some information that you need to maintain separate format for Welding process validation.

A- DETAILS OF EQUIPMENT USED FOR VALIDATION
The process equipment's used for the validation shall be proven capable of performing the task for which they were designated

B- QUALIFICATION OF PERSONNEL INVOLVE IN THE VALIDATION
Welding Engineer / QC engineer shall ensure that only qualified personnel are assigned for the respective process, includes the weld overlay operator qualification

C- CRITERIA FOR REVIEW AND APPROVAL OF THE PROCESSS
Criteria for review and approval of the process shall be based on the criteria requirement specified in the appropriate qualification code and standard.

D-USE OF SPECIFIC METHOD AND PROCEDURES
WPS, PQR, Materials used, code requirements, specifications, procedures, inspection and testing, defining the acceotance criteria and its reference documents

E- REQUIREMENTS OF RECORDS
Equipment Operation Manual
Maintenance Records of Equipment
Calibration records for control pannel
Qualified WPS & PQR records
Operators Qualification records
Inspection & Testing records


Hope this clarifies your query and proceed further.

NEILASHKUMAR.P
WELDING ENGINEER


On Thursday, 31 August 2017 9:06 AM, Nachhattar Singh <nachhattar1947@gmail.com> wrote:


Dear Experts
 
I am required to submit to the client as to how the "VALIDATION OF THE WELDING PROCESS FOR
THE HARD FACING AND SEAT RING WELDING OF THE GATE VALVES" will be done. Following has already
Been complied and submitted but the client wants some more to be done:-
 
01.   WPS is accepted as submitted.
02.   PQR based on the WPS is in place and accepted.
03.   Heat treatment is not the requirement.
 
Please advise what else should be done, give the reference of such requirements.
 
Thanks in advance
 
NS Gurm
 
PLEASE THINK BEFORE PRINTING
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...