Skip to main content

Re: [MW:26771] Pitting corrosion in Duplex material

Thanks all for the quick response..

Regards,
Aby

On Wed, Aug 30, 2017 at 5:20 PM, Aby Jose <abycscec@gmail.com> wrote:
Dear Goswami sir,

The temperature of test was 40 degree celcius. Heat i/p for TIG was from 1.5 to 2.2 and for MAG 0.65 to 0.9. Pitting corrosion was observed both on root and in cap. But more in cap.

Regards,
Aby

On Wed, Aug 30, 2017 at 2:48 PM, pgoswami <pgoswami@quickclic.net> wrote:
What's the  temperature for pitting corrosion test? What're the recorded welding parameters including heat input?
Appreciate your response. 
Thanks. 

Pradip Goswami. 



Sent from my Bell Samsung device over Canada's largest network.

-------- Original message --------
From: Aby Jose <abycscec@gmail.com>
Date: 2017-08-30 03:40 (GMT-05:00)
Subject: [MW:26765] Pitting corrosion in Duplex material

Dear experts,

Here I am preparing WPS for Duplex material using robotic welding machine. The details are as follows.

Material designation - SA 790 UNS S32205
Pipe dimension - 4",  6 mm thick
Welding process- TIG(Root), MAG(fillup & Cap)

After the PQT while doing the pitting corrosion test it got failed. The pitting corrosion test was done as per ASTM G 48. 

For TIG welding earlier I had used 98% Ar + 2% H2 as shielding gas. Now I have changed it to 98%Ar + 2% N2. 
For MAG welding pulse method is used. Shielding gas used is 98% Ar + 2% CO2. Purging gas used is 99.997 % Ar. 
Heat i/p calculated is within the range 0.6 to 1.5. Also the interpass temperature was below 120 degree. What else can be the reason for Pitting corrosion? It came more in the capping. So I am worried about the shielding gas used for MAG. Which other shielding gas can I use for the MAG welding of duplex material??

Regards,
Aby K Jose
QA/QC Engineer
Qatar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...