Skip to main content

RE: [MW:25695] Tube to Tubesheet Joint

No. You cannot use 10.0mm PQR for tube to tubes heel joint.


On 15 Nov 2016 02:07, "John Henning" <jhenning@deltak.com> wrote:

Minor adjustment - ASME Section VIII Div. 1 does not mandate tube-to-tubesheet mockup for qualification  - however Division 2 does.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of George Dilintas
Sent: Sunday, November 13, 2016 7:28 AM
To: Meghanadh K
Subject: Re: [MW:25676] Tube to Tubesheet Joint

 

Taking into account that your Pno is 43 you may benefit of the provisions of  QW 202.4.

However before take a final decisions check the requirements of QW 202.6

 

2016-11-12 16:23 GMT+02:00 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com>:

Hi

 

Assuming your construction code is ASME SEC VIII div.1, 

You will have to carry out a separate tube to tube sheet mock up qualification.

Refer ASME SEC IX and SEC VIII Div 1 for details.

Also tube to Tube sheet mock up qualification will be mentioned in your approved QAP

 

 

 

REGARDS

 

 

PREM NAUTIYAL 

9769316004

 

 

 

 

 

 

Sent from my Samsung Galaxy smartphone.

 

-------- Original message --------

From: pankaj phuse <pankaj.phuse@gmail.com>

Date: 11/11/2016 16:15 (GMT+05:30)

To: Materials & Welding <materials-welding@googlegroups.com>

Subject: [MW:25662] Tube to Tubesheet Joint

 

Dear Experts,

 

Need your guidance on the following:

 

We have tube to tube-sheet joint having Groove + Fillet Weld without grooves & expansion. (Tube-2.7mm, Tubesheet-45mm, P No.43 to P. No.43)

 

I have PQR qualified on plate 10mm Thk. (P No.43 to P No.43, Qualification Range - 1.5 to 20mm).

 

Can I use the same WPS for this joint or we have to qualify new procedure.

 

Procedure qualified as per ASME Sec.IX.

 

Need clarification with reference to clause number.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3vk1jfblmfkop6qg13yd2on8.1478960138453%40email.android.com.


For more options, visit https://groups.google.com/d/optout.



 

--

Dr. Georgios Dilintas,

Dipl. Ing. In Aeronautic and Space Engineering

Ph.D in Mechanics of Solids - Computational Mechanics

A.I.S, A.N.I, IRCA Lead Auditor

Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CvE1uMPy%3D9tkh3nNYYM1LCpvxobZhbQWbZivqGgJXMXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MWHPR03MB281676B9A3440FA3FA7F050EA1BC0%40MWHPR03MB2816.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD1AzTQzozVFNp05ThrFSEKD_0KLqwn-SAKgTLMhL7WsGrEXaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...