Skip to main content

RE: [MW:23226] Hydrotest after Addl. Nozzle provision

 

As adding/replacing 10" nozzle is not a major repair so no engineering evaluation is required but please refer 12.3.2 of API 653 Addendum 2012 of fourth Edition for more details.

 

Faisal Shahzad Meer

+966 - 553919249

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kunal saini
Sent: Monday, July 27, 2015 6:17 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:23218] Hydrotest after Addl. Nozzle provision

 

Dear faisal,
I have the same case but is there any need to get any design evaluation for the same modification.

On Jul 27, 2015 7:36 PM, "Faisal Shahzad Meer" <fmeer@gccksa.com> wrote:

This clause is in API 653 not in API 650.

3.19 definition of major alteration/major repair.

 

Regards

 

Faisal Shahzad Meer

+966 - 553919249

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Thota Kishore
Sent: Monday, July 27, 2015 9:17 AM
To: materials-welding
Subject: Re: [MW:23210] Hydrotest after Addl. Nozzle provision

 

Sir,
Thank you very much for the information. Also pls let me know the clause in API 650, not to do Hydrotest after modification below 12" nozzle.

On 26-Jul-2015 12:13 pm, "yakoob khan" <yakoobengineer@gmail.com> wrote:

Dear kishor,

Hydrotest condition for the tank made up by API 650 is the requirements of carring out major repair means minimum 12 inch nozzle replacement or addition under the working height of liquid.
It means you don't have to do Hydrotest just do the pneumatic at 15 psig for reinforcement pad.

On Jul 26, 2015 9:22 AM, "Thota Kishore" <krish.royal18@gmail.com> wrote:

Dear Members,

We have constructed API 650 storage tank (28m Dia x 16.5m HT), hydro test, painting and calibration has been completed. But now client requires additional 10" nozzle in the tank. 

If i provide 10" nozzle now, whether i have to do hydro test again or pneumatic test is sufficient. If so, please let me know the clause with Ref. Std.

Kindly suggest me.

 

Thanks in Advance.

Regards,

Kishore Thota

9951141681

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALpPUFuH1JPwGPD8PJb1GhEzup3GBkuBFT3uuHsMSQ3Y1Ug3Hw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABhShnbbwV8OXSTNWJ6f0okv3tj-P-Uiiq6hb%2B1PMaE9rTz%2B3w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALpPUFvOAJHX9MTkeLX5_-B%2BBwXq4RibKPnd1q7KKbehxgZZOw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This e-mail and any attachments may contain confidential and privileged information. If you are not the intended recipient, please notify the sender immediately by return e-mail, delete this e-mail and destroy any copies. Any dissemination or use of this information by a person other than the intended recipient is unauthorized and may be illegal.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/A09A3236B96A6E4290C41417C8A0147E0ADC5751%40GCC-MAILBOX.gcc.local.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGWuPA%2BLcmgUNhkvnOh8SH-JosA5Fbun0KTQ-6sXvy5ooe2%2BXw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...