Refer to ASTM A6 AND A 20 for details regarding product analysis

On Mon, Jul 13, 2015 at 9:29 PM, Umar Makrani <firoz.makrani@gmail.com> wrote:
In technical delivery conditions the client mentions 
"S19. Restricted chemistry: Carbon Max 0.2% and Vanadium Max.XX% restricted for heat and product analysis,"

In context of SA20, should the supplementary requirement S2 be invoked?

 

 

Thanks & Regards

 

Firoz Ahmed R. Makrani, PMP®

On 13 Jul 2015, at 7:17 pm, Dark_Horse <srinivas.sreeram@gmail.com> wrote:

Product analysis is always on basis of Heat No and it is done on sampling basis.   In case of coils, it is done from drawing sample from both front and tail end of the coil.  for it is illogical to take it from centre of the coil !!!.
If buying from a trader, possible plates may  belong to different heat, then buyer to advice whether they want 100% testing or random samples.

sreeram

On Thursday, July 9, 2015 at 1:11:45 PM UTC+4, Umar Rashid Makrani wrote:
Further,
The client requirement is" S19. Restricted chemistry: Carbon Max 0.2% and Vanadium Max.XX% restricted for heat and product analysis, can I interpret this as a supplementary requirement S2of SA20?

On Wednesday, July 8, 2015 at 1:35:52 PM UTC+3, Umar Rashid Makrani wrote:
Dear Mentors,
For Material ASTM A516 Gr 70 the client requirement is based on product analysis. Does that mean that all plates shall be tested for product analysis? or certain plates from that heat is enough to report that as product analysis.
Thanks in advance for your kind advise if possible with citation.
Best regards,
Umar.

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/NDLX5-JcODk/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/825d64ec-6610-4c26-bc2f-b715b0f09f74%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/11598EFD-EDBA-4DBD-9241-0E966A0DDD34%40gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC-DWStukOiRuN9mXhNLw977Bz%3D%3Dbh9iwhOKaSQ6A4u7tz%2BSVA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...