Hi Nitin,
 
When it comes to consumables for Grade -91 steel, you do not have many choices.Only a handful names.Please see the extracts from a list of approved vendors for such electrodes, from a large Power Plant Design and Fabrication Organization in India.I believe products of all these manufacturers are available in India. In addition there may be indigenously manufactured brands from ADOR and D&H.
 
By the way the highlighted specification E-9013 is not correct. Grade 91 electrode comes with 3 -AWS designations
  • E9018-B9
  •  E9016-B9
  •  E9015-B9
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 
       
SFA 5.23 E B9 BOHLER SCHWEISSTECHNIK AUSTRIA BOHLER C9MV-UP
SFA 5.23 E B9 BOHLER THYSSEN SCHWEISSTECHNIK THERMANIT MTS-3
SFA 5.23 E B9 ESAB INDIA LTD.,CHENNAI OK 13.35
SFA 5.23 E B9 METRODE PRODUCTS, U.K. 9CrMoV-N


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of nitin jain
Sent: Thursday, July 02, 2015 1:53 AM
To: materials-welding@googlegroups.com
Subject: [MW:23126] Re: P91 WELDING ELECTRODES

Which are the Good Companies Manufacturing and exporting P 91 welding rods and Wires and TIG fillers from USA/ Canada/ Europe??? not many i believe

Metrode and Bohler selling in India but not any other heard. Can someone guide quality manufacturuers of P 91 TIG/ FCW and welding rods
contact: nnittinn@yahoo.com

On Thursday, June 9, 2011 at 8:27:13 PM UTC+5:30, Eng/ Mostafa Kamel Hussein wrote:

Can i weld the P91 with E9018 or E9013 instead of E9015-B9? and why?
i need the answer urgently 

Regards
SaSa

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/25d9385d-9119-408a-8f4a-a8944050be83%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...