Re: [MW:23225] Re: EBW in titanium for T>50mm

If I remember correctly, L&T Hazira did titanium matl heat  exchanger, wall thickness 9 or 12 mm in 1995 in light fabrication shop with TIG process.
Regards,
S.SENTHILKUMAR



On Monday, 27 July 2015 2:13 PM, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:


Sir,
Thank you for this information. As far as GTAW is concerned we have much of expertise.
We had also enquired at DRDL,HAL etc. But they regreted.
For BARC, haven't enquired as I didnt get any contact. If u have any pl share.
If that also doesn't work, what u suggest? I think SAW to be carried.
Thank you.
Hrushikesh H Sangamnerkar
On Jul 27, 2015 10:50 AM, "Muthukrishnan Sivaramakrishnan" <smkro3@gmail.com> wrote:
Dear Mr.Sangamnerkar,

I doubt about the capabilities of EBWs available in India to meet your demand .For 3 to 4 meter diameter you have to use partial vacuum EBW system which works in open air .Such a facility was demonstrated by SCIAKY ,Frnace in 1776 if I remember correctly during my training at this facility and I participated in this programme. We welded 80 mm thich SS 316 vessel of dia same as yours .In this system the EBW gun will move along the vessel covering the joint area with a special partial vacuum system . OSAKA university people developed another machine in which the vessel is kept in a vacuum room and the beam is impinged on the vessel mounted on a rotary positioner .

For your immediate use please use normal TIG welding and a roller positioner rotate the vessel. Please inform your location ,vessel dimensions and code requirement .If you need an welding expert to visit you for procedure qualification with TIG please inform .

Regards,
S.Muthukrishnan

On Sun, Jul 26, 2015 at 12:09 PM, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
I have shell Dia. Of 3-4 meters. Are they doing EBW with the above mentioned diameter also?
Hrushikesh H Sangamnerkar
On Jul 25, 2015 8:06 AM, "Hrushikesh Sangamnerkar" <hrushi612@gmail.com> wrote:
Gm all,
Anyone experienced in EBW of titanium?
Pl share. Suggest any vendor who has this facility, if any.
Hrushikesh H Sangamnerkar
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2o_6y2__XcWzAhXo6f_JvTOLCJZFxeH%3D-V%3DiyUK%2BWggbA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAB-sOHSUmmw08O4P4J-nF205PohdFHpJECmT134aMC-7oXzQw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rzpXVXGSVFZasFdRMMoYMseXUd9SbKpFZNzhiN4NtUoQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...