Tuesday, May 5, 2015

[MW:23204] how prepare Wps &pqr for ss304cladded with hastelloy (c22)

Hi to all,
                 i've to prepare and approve wps&pqr for ss304cladded with hastelloy (c22).Can we use 304l electrode for ss304 side and Nicrome-10(c22) electrode foe c22 side.
i need explanation from code ..i.e how to follow in ASME IX
I attached drawin also plz check
thanks
 regards
hari krishna

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f41dcf30-d9a7-4dfc-bbe0-1718a998b715%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone