[MW:22997] Welding filler wire/Electrod for A 105 to A335 P11

Dear Experts,
 
Can any one suggest the suitable welding filler wire and electrode for welding CS A105 to A335 P11.
 
Regards
 
B Osare
N F L Vijaipur
 
Sent: Monday, March 23, 2015 2:13 PM
Subject: [MW: 22996] Re: 20405] ASME Sect IX-QW-405-Position Qualification Ranges [GroupMail]
 
Hi All
Referring to ASME Sec. IX 2013, understand that QW-405.4 applies to hardfacing and corrosion resistant overlay.
 
1) Can anyone clarify the difference between QW-405.4 para (a) and para (c)?
2) Will overlay qualification with 2G up-hill progression qualifies Flat position?
 
Thanks and Regards
Harikrishnan

On Wednesday, March 26, 2014 at 2:52:41 AM UTC+8, John Henning wrote:

Your reasoning is flawed and your answer incorrect.

 

Another example of reading the QW-4xx variables out of context.

 

QW-405.2 typically applies to general process qualification (groove welds, etc.). 

QW-405.4 apples to special process qualifications (Hard facing or corrosion resistant overlay).

 

These two variables are never called out together.

 

Regarding the application of supplementary essential variable QW-405.2, I suggest you read Interpretation IX-81-24 reply to question 1 states :

 

Reply (1): When applying QW-405.2, any position not involving the vertical uphill progression will qualify for all positions, except those involving the vertical uphill progression. Any position involving the vertical uphill progression win qualify for all positions, including those involving the vertical uphill progression. For example, qualification on a test coupon in the 2G position will qualify 4G and 5G downhill, but not 3G uphill. Qualification on a test coupon in 3G uphill progression will qualify 4G, 6G uphill progression, and all other positions.

 

 

John A. Henning

Welding & Materials

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Anban
Sent: Tuesday, March 25, 2014 3:49 AM
To: material...@googlegroups.com
Subject: [MW:20405] ASME Sect IX-QW-405-Position Qualification Ranges

 

Dear Experts

 

Position only a Supplementary essential variable (ie when CVN-Impact test required).

 

QW-405.2 A change from any position to the vertical position uphill progression. Vertical‐uphill progression

(e.g., 3G, 5G, or 6G position) qualifies for all positions. In uphill progression, a change from stringer bead to weave

bead. This variable does not apply when aWPS is qualified with a PWHT above the upper transformation temperature

or when an austenitic material is solution annealed after welding.

 

QW-405.4 (a) Qualification in the horizontal, vertical, or overhead position shall also qualify for the flat position. Qualification

in the horizontal fixed position, 5G, shall qualify for the flat, vertical, and overhead positions. Qualification in

the horizontal, vertical, and overhead positions shall qualify for all positions. Qualification in the inclined fixed position,

6G, shall qualify for all positions.

 

I'm looking at some of the WPS/PQRs received from Vendor.

PQR state that Position Tested/Qualified- 1G

WPS state qualified for all groove and fillet positions?

CVN Tested at -30 deg C.

 

Based on QW-405.2 & QW-405.4- 1G does not qualify all positions.Only qualified for 1G & 1F.

 

Plls explain how "This variable does not apply when aWPS is qualified with a PWHT above the upper transformation temperature

or when an austenitic material is solution annealed after welding." relevant to Positions.

 

 

Pls shine some light on this. Thank You.

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bee3a3dd-1a95-4ec0-8149-415cae9579a8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...