Re: [MW:22985] Re: Tolerance for Dog leg

The relevnt tolerances have been illustrated in PFI ES3
 
Thanks,
Ash

On Tuesday, February 12, 2008 at 6:44:53 PM UTC+7, quality wrote:

It seems to be a process piping with design code ASME 31.3.

If the fabrication/ construction code is ASME B 31.3, it also permits a miter bend upto 3° is acceptable (ref ASME B 31.2 Article 304.2.3).

In other words, a deviation/ deflection upto 3° can be considered as straight pipe & does not effect the design conditions (unless otherwise this tolerance is over ruled by designers with a strict requirement for maintaining a slope or aesthetic appearance is important than the allowable tolerance). Then do not look further for acceptance tolerance. Rectify the joint & make it straight.

best regards,

Sanjeevan 

Gulf Petrochemical Services, Muscat, Oman 

 

----- Original Message -----
Sent: Tuesday, February 12, 2008 2:37 PM
Subject: [MW:565] Re: Tolerance for Dog leg

Here by attached the photo related to typical dog leg.
We are facing this problems in construction stage of plant piping. Allowing 3 Deg as tolerance appears to be more liberal and in lines like relief /blow down where slope of the line is  to be maintained process point of view. 
Thank you very much to all of you for your prompt reply.
 
Regards
 
Srs reddy
Saudi Aramco
 
 
 
 
 
On 2/11/08, Shyam Herur <herur...@gmail.com> wrote:
Can you specify the pipe spec and what it is used for ? Since you are referring to "line pipe" I presume its the pipe covered in spec API 5L. However I did find an abstract which  goes" usually out of straightness of pipe usually follows a log normal distribution with diametre, and, as would be expected the larger the diametre of the pipe, the straighter is the pipe. API 5L allows  24mm in a 12m joint. usually it is possible to obtain pipe to 12mm in 12m. to reduce total cost over specification of straightness should be avoided".
 
also refer to API 5L for further details.

 
On 2/11/08, Sankepalli R.S.Reddy <sankepall...@gmail.com> wrote:
It is the out of straightness of line pipe. The out of straightness may be due to weld distortion at joint locations or due to improper fitup.
regards

 
On 2/11/08, Raghuram Bathula <raghura...@gmail.com> wrote:

Can you please explain the term Dog leg, i have no idea what it is?
Is it a term related to steel structure? type of stair case
arrangement?

On Feb 11, 7:39 pm, "Sankepalli R.S.Reddy"
<sankepalli.rsre...@gmail.com> wrote:
> *Dog leg or out of alignment of line pipe:*
> **
> Can any body gives permissible tolerance for Dog leg. Whether any standard
> is covering this tolerance.
>
> Thanks and regards
>
> S. Rama subba reddy
>
> Inspection Engineer
>
> Khursaniya Gas Project, KSA
>
> Bldg 7, Cu 1
>
> Ph no: 6770120







No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.516 / Virus Database: 269.20.2/1272 - Release Date: 11/02/2008 05:28 c

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39e2e544-ea0b-4015-9d58-d49dfdc3dfed%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...