Skip to main content

Re: [MW:22924] FCAW Process Filler wire E71T-1C does this come under low hydrogen electrode category?

Dear PKM,
Its not coming under Low Hydrogen Electrode category.

Regards,


 Muniyandi Chithiran MBA.,MIIF,
AWS CWI,
ISO 9001,14001,17025,27001,OHSAS 18001 Auditor,
NDT Level II,

Mobile: 0091 95855 40965

Just because a relationship ends doesn't mean two people stopped loving each other.They just stopped hurting each other.

On Mon, Mar 2, 2015 at 1:29 PM, PK M <pkmqaqc@gmail.com> wrote:

Dear Sir,

 

Good day,


FCAW Process Filler wire E71T-1C does this come under low hydrogen electrode category?

 


ASME Sec IIC-SFA 5.20

 

A8.2.4 Most flux cored electrodes deposit weld metal having diffusible hydrogen levels of less than 16 mL/100 g of deposited metal. For that reason, flux cored electrodes are generally considered to be low hydrogen. However, some commercially available products will, under certain conditions, produce weld metal with diffusible hydrogen levels in excess of 16 mL/100 g of deposited metal. Therefore it may be appropriate for certain applications to utilize the optional supplemental designators for diffusible hydrogen when specifying the flux cored electrodes to be used.

 

Question no -01

 

In the engineering drawing for welding the anchor chair of atmospheric storage tank in the field, it is specified to “Weld with low hydrogen electrode”.

 

Can we weld with FCAW process using E71T-1C filler wire, ASME Sec IIC-SFA 5.20 for above mentioned application? The EN10204 3.1 certificate for the filler wire shows hydrogen test results performed on the deposited weld metal, a maximum of 3.0 ml/100g.

 

Question no -02

 

Is there any difference between “low hydrogen weld deposit” and “low hydrogen electrode” in the light of ASME Code?

 

 Note:-

Also Find attached files..

 

 

Please kindly provide code reference...

 

Thank you.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_neZ4YX676Ra1%3DZ5iGYc6d-w2u-%2B2gWZE1rgBFU5Vro26g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMJSSYkDZskPp7OdRtG4k%3DAaB%2BKXtNE0Freb_PBtHF-URt0%2Bcw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...