Group number fall under sup. Essential variables. So unless there is no impact requirement you can be used. For severe cyclic group number also became essential variable.

Regards,
Venkadesh

From: Muthu Samy
Sent: ‎04/‎12/‎2014 16:42
To: materials-welding@googlegroups.com
Subject: [MW:22457] Combination of PQRs

Dear Friends,

I have two WPSs in which base metal qualified with  P1 Gr 1+P1 Gr 1  PQR A Process SMAW+SAW
                                                                                    P1 Gr 2+P1 Gr 2  PQR B Process SMAW+SAW

The query is I need to weld the P1 Gr 1 with P1 Gr 2. Is it possible with any one of these WPSs?. 

வாழ்க வளமுடன் என்றும் நலமுடன்

LOVE EVER HURT NEVER

Muthusamy.S




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...