Dear friend,

Following is a part of QW-403.5:

"If, however, two or more
qualification records have the same essential and supplementary
essential variables, except that the base metals
are assigned to different Group Numbers within the same
P‐Number, then the combination of base metals is also
qualified."

Regards

On Thu, Dec 4, 2014 at 12:58 PM, Muthu Samy <jenieragav@gmail.com> wrote:
Dear Friends,

I have two WPSs in which base metal qualified with  P1 Gr 1+P1 Gr 1  PQR A Process SMAW+SAW
                                                                                    P1 Gr 2+P1 Gr 2  PQR B Process SMAW+SAW

The query is I need to weld the P1 Gr 1 with P1 Gr 2. Is it possible with any one of these WPSs?. 

வாழ்க வளமுடன் என்றும் நலமுடன்

LOVE EVER HURT NEVER

Muthusamy.S




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...