Skip to main content

Re: [MW:22625] Material Certificate EN 10204-3.2 without TPI Witness

Hi,

only 3.1 required 3rd party inspection /Witness  and stamp not 3.2.

3.2  is manufacturer testes the material in 3rd party lab  no need for 3rd party witness until customer specified to do so.


Regards,

K.Venkateswaran

From: Afshin <ar.mermco@gmail.com>
Sent: Sun, 14 Dec 2014 15:28:46
To: materials-welding@googlegroups.com
Subject: [MW:22564] Material Certificate EN 10204-3.2 without TPI Witness
Dear All,

I have a question about difference between material certificate and inspection certificate both grade 3.2, I am doing business in the field of pump and my customer asked for inspection certificate type 10204 3.2, but pump package includes motor, pump, base plate, coupling and etc. I think inspection certificate means presence of inspector during performance test and declare that package manufactured based on project specification and order.

Regards,
Afshin 

On Monday, December 9, 2013 9:49:56 PM UTC+3:30, BK wrote:

Dear Experts

As per project Specification the Material Certificate requirement for primary structural steel (S355 G8 M) is EN 10204-3.2. 

We received Mill Certificates along with material and in that it is mentioned "Certificate as per EN 10204-3.2" but the Third Part Inspector from Client and Third Party Inspector from EPC contractor REVIEWED and STAMPED at manufacturer's location. And no any evident on Mill Certificate that the tests were witnessed by any third party inspector, but it is stated 3.2 Certificate.

By Definition of 3.2 Certificate Third Party Inspector shall have witnessed the tests stated in the certificate. 

Please clarify the following:

1. Is it acceptable 3.2 certificates without Third Party Inspector WITNESS ? 

2. On what basis manufacturer declaring 3.2 ?

3. Is it acceptable if manufacturer declared 3.2  without showing any evidence. 

Regards
BK 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group';s bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...