RE: [MW:22307] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

Hi Ahmed,

 

Thank you (Shukran) for the valuable information. One more question, this mix of argon and nitrogen, what ratio's would be optimum.

 

We are Tig welding material that is 0.15mm thick. We typically weld with about 18A, and a linear speed of 50mm/sec. At this point in time we are purging with 100% Argon.

 

Regards,

 

Naasief

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ahmad el-sharkawy
Sent: 20 November 2014 09:21 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22304] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

 



On Wed, Nov 19, 2014 at 11:13 PM, Ahmad el-sharkawy <ahmad.sharkawy88@gmail.com> wrote:

dear Noe Mota mixture of argon and nitrogen is the best gas purging for welding duplex and super duplex stainless steel


 

 







On Wed, Nov 19, 2014 at 10:34 PM, Ahmad el-sharkawy <ahmad.sharkawy88@gmail.com> wrote:

dear Naasief Navsa use mix of argon and nitrogen and use low heat input.

 




--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI "
14072901.
ASNT LEVEL II "
RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.

PREPARING MASTER DEGREE IN WELDING ENGINEERING.




--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI "
14072901.
ASNT LEVEL II "
RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.

PREPARING MASTER DEGREE IN WELDING ENGINEERING.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.




This email has been scanned for email related threats and delivered safely by Mimecast.
For more information please visit http://www.mimecast.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...