RE: [MW:22005] WELDING JOINT A335 P91

Hello Expert,

 

I recommend to use ER9S-B9 and E9018-B9 which will match the chemistry of A335 Gr P91 material.

 

Bala Nechur,

Corporate QA/QC Manager

Phoenix Industrial,

Office: 780-428-3130  Ext 736

Cell: 780-204-0239

Fax: 1-866-211-3193

Toll Free: 1-866-778-3130

Email: bala.nechur@phoenixindustrial.ca

                                                                                                     

The information transmitted is intended only for the addressee(s) and may contain confidential, proprietary and/or privileged material, unauthorized review, copying, distribution, taking of any action in reliance upon or disclosure is strictly prohibited. If you are not an intended addressee, please delete this message, including attachments immediately

 

Please don't print this e-mail unless you really need to.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pras ari
Sent: September-26-14 10:16 PM
To: materials-welding@googlegroups.com
Subject: [MW:22004] WELDING JOINT A335 P91

 

Dear Experts,

We have study case, on our project (steam power plant project), there was any welding joint i.e. welding pipe A335 P91 to A335 P91 with filler metal GTAW ER90S-B3 + SMAW E9015-B9 and PWHT 750 C with holding time 2 hours.
Please advise us, what impact these welding joint for strength and lifetime if compare with GTAW ER90S-B9 + SMAW E9015-B9 and PWHT 750 C with holding time 2 hours.
What can we do and the solution this case.

Thanks and regards
Winarko
QA/QC Welding Inspector
+6281288300094

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...