Monday, September 22, 2014

Re: [MW:21968] Re: Pqr qualification 5g

Dear All,

Welding position is non essential variable for WPS /PQR qualification. You can use any WPS for Welder qualification.


Vikas Rana

On Sun, Sep 21, 2014 at 3:39 PM, AHMAD&MOHAMAD REDA <amreda2006@gmail.com> wrote:
dear sir
refer to ASME IX qw 203 for the limits of qualified positions for the procedure
AND u can qualify your welders in any positions with PQR listed  with same material.

OUR BEST REGARDS

AHMAD AND MOHAMAD REDA

01223964394&01223932379

HEAD SECTION QA-QC

PETROJET - EGYPT


On Thursday, 18 September 2014 14:32:13 UTC+3, Narender Reddy wrote:
Dear experts

Q:1) I have 5g PQR (PIPE)can i use that pqr for 6g  welder qualification test with same material specification

q:2) I have 5g PQR qualified with 4 inch (PIPE)can i use that pqr for 6g fo 2 inch  welder qualification test with same material specification

Q:3) I have 3g PQR (plate) can i use that pqr for 2g,4g  welder qualification test with same material specification


Please reply on this

Best regards
Narender reddy.M

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...