Hello,
Materials with Z properties simply means improved Tensile Properties in the Z direction (Through thickness of the materials) which also has a resttriction on the level of imperities (Sulphur Content). it could be Z15, Z25 or Z35 but whatever it is, it does not required special Electrode or seperate WPS if all other things are equal. Z Materials are recommended when there will be heavy welding on the through thickness of a materials.
Regards,
Rems Okonkwo.
IWE Nigeria
On Mon, Sep 22, 2014 at 8:54 AM, Airon <isacnewt@gmail.com> wrote:
Does Z Grade plate welding needs separate WPS ? Does it require any special Electrode?--Material is D36 Z grade plate.What are things to be taken care of when welding this to normal plates. Electrodes. WPS etc..
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments