[MW:22005] Re: QW 406 , preheat maintenance

Dear Sir,

Preheat maintenance, according to ASME IX,  is not post heating.
If it should be carried out NDT or not sure welding joint perfect, you can cool down before PWHT.
Preheat maintenance means that you do not cool down before perform PWHT



On Friday, June 20, 2014 7:29:50 PM UTC+7, rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA wrote:

   Dear sir
               thickness and  OD : 323 od* 70 mm thk
               welding process : GTAW+SMAW
               Material : SA106 Gr B
               Preheating : 100 deg c
               weld deposition : for GTAW : 4 mm, SMAW : 66 mm


   Question  :
                  1) Is the preheat maintenance (post heating ) is required for  above material
                  2) If YES, what is time and temp  plz send the back up
    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...