Sunday, September 21, 2014

[MW:21961] Re: Ovality check for 32" pipes

Dear swapnil sonavane

Make a straight bar of steel equal to the internal dia. Of pipe -

By using radiography film (roll) to insure circularity, draw a circle inside the pipe -

-run the bar on the circle when it is stuck u have the min. dia. And when there is a difference between the bar and the internal circumference measure it.

Normally u will find the max. ovality in the first row of storage  

 

OUR BEST REGARDS

AHMAD AND MOHAMAD REDA

01223964394&01223932379

HEAD SECTION QA-QC

PETROJET - EGYPT 


On Thursday, 18 September 2014 11:28:07 UTC+3, swapnil sonavane wrote:

Dear Experts,

Pls. advise the accurate method for checking ovality of 32" pipes.

Regards,

Swapnil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...