Monday, July 1, 2013

[MW:18069] out of straightness


 dear all
      our construction code is B31.3, during line checking for the test pack i found that line is not straight (out of straightnees) upto 4-5 mt  ,after that line is deviated from it origin and continue, i am looking for acceptance criteria for it but i did not find it in code and project procedure for fabrication
     so kindly any one can explain me about this issue./where it is mention
 
Thanks & best regards.
Mohammad Jawed Anwar .
(welding inspector)
Mob no #  +966569799776.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35346] Cast-iron welding