[MW:17145] Opening on longitudinal weld of the run pipe per ASME B31.3

Interesting, i do agree we have to avoid as far as possible this intersection, however in my opinion it may not be necessary to recalculate the RF pad details, as the product of SEW is already taken care while internal pressure design calculations per 304.1.2.

any example where this will differ? i mean selection of S only

i have changed the subject line to suit this topic now.

On Monday, March 18, 2013 12:09:43 PM UTC+5:30, KVH wrote:
Please refer 304.3.3 (Reinforcement for welded branch connection) of ASME B 31.3 ( on the assumption as your construction code)

Refer the definition of t=Pressure design thk of pipe. The thickness calculation for reinforcement pad is based on whether it is intersecting a longitudinal weld or not.

So as the code has given of both options (with intersecting and without intersecting), the welding is acceptable as per my opinion.

Normally the thickness of pad and welding details which is given in project standards will be on the assumption that the branch is not intersecting a longitudinal weld, If it does then the designer has to recalculate the reinforcement pad details.

As a good engineering practice, it should be avoided and it is the prime responsibility of Fabricator and site engineer to avoid this.

Please see further opinions from experts of this group before coming to a conclusion.



On Sun, Mar 17, 2013 at 2:59 PM, Anil Hegde <nott...@gmail.com> wrote:
Dear Expert ,

We have a 36 inch pipe which is welded type ,On it We have 12 inch connection which is coming on the ( long seam ) of the pipe .

Is There any code which says we can or cannot do welding on long seam of the pipe .

Requesting you for your positive feedback .


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...