Back strip is nothing to do with any defects for RT interpretation, as long as welder is skilled & experienced.
-- On 5 August 2012 15:09, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Back strip will not be considered for RT interpretation.CVR--
On Wed, Jun 20, 2012 at 11:54 PM, eng ahmed <eng_ahmed450@yahoo.com> wrote:
--Dear AllI had problem to weld pipe A53GrB using carbon steel back strip techniqe in RT interpretation,May i know the defects of welding the pipes using carbon steel back strip A109 type by GTAW process.Best Regards
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment