Saturday, August 4, 2012

Re: [MW:15021] Re: Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE

Dear Mr. Alam,
 
Please go through
 
 
regards.
 
Arun S Das
 

From: c sridhar <sridhar305@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Friday, 3 August 2012 1:33 PM
Subject: Re: [MW:15018] Re: Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE
Mr. Sahid Alam,

If we understand the process, you are doing spiral welding of pipes(or) pipe welding in 5G position with pipe on rotation.

Short cut lengths  of pipes beyond 2 meters are allowed for welding. If they are  circumferential joints, make sure that, the pipe seams are oriented by 90 deg.  Hence pipe lengths of 7 mts and above should not create  any problem at all.

sridhar.

From: Sheldon <xiaochenzhu@gmail.com>
To: materials-welding@googlegroups.com
Cc: engineer_makes_world@yahoo.co.in; Abdul.Chachar@WorleyParsons.com
Sent: Thursday, 2 August 2012 10:52 PM
Subject: [MW:15015] Re: Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE
Hi there,
 
I am wondering what is the difference between API system PSL 1 and CSA system Category I? Also, the PSL 2 and Category II? The only thing I aware is the temp. for Impact test which is 0 deg. c for PSL 2 but -45 deg. c for Category II. is that all?
 
Cheers guys!
 
Sheldon
 
 

On Monday, June 27, 2011 5:41:35 PM UTC-6, sajidalam mohd. wrote:
DEAR EXPERTS
                 WHAT IS DIFFERANCE BETWEEN PSL1 & PSL 2 CARBON STEEL PIPE.
 
I AM DOING INSPECTION FOR PSL2 CARBON STEEL PIPES (BY SAW PROSESS AS PER API5L).
 
OUR PIPE'S LENGTH ACCEPTANCE CRITERIA IS 12 METER TO 18 METER.
 
 
MANUFACTURER HAS SO MANY SHORT LENGTH PIPES LIKE AS 8 METER, 7 METER & 10 METER.
 
HE WANTS TO JOINT TWO SHORT LENGTH PIPES BY SMAW PROCESS.
 
I WANT TO ASK THAT IF MANUFACTURER IS JOINING TWO SHORT LENGTH PIPES THAT PIPE WILL BE ACCEPTED AS PER API5L FOR PSL2.
 
MANUFACTURER IS SAYING THEY HAVE APPROVAL FROM CLIENTS ABOUT ABOVE MENTIONED ISSUE.ME SHOULD GIVE RELEASE FOR THAT PIPES OR NOT.
 
IT IS ALLOW OR NOT/AND WHERE IT IS MENTIONED THAT FOR PSL2 PIPES IF LENGTH ACCEPTANCE CRITERIA IS MENTIONED BY CLIENTS/API5L AFTERTHAT MANUFACTURER WILL JOIN TWO SHORT LENGTH PIPE AND HE WILL PROCESS THAT PIPES AS  PER PSL2  PIPES.
 
 
REGARDS
MOHAMMAD SAJID ALAM
INSPECTION ENGINEER
KUWAIT
 
 
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...