Thursday, August 2, 2012

Re: [MW:15012] Stress relieving cycle for 6 mm welded plate

Please refer UCS 56 in Sec VIII Div.1
No PWHT is required for 6mm thickness weld P1 materials.
Also refer your client technical specifications.
 
Regards
 
Prem Nautiyal


--- On Thu, 8/2/12, Gopalakrishnan G <gopal2408@gmail.com> wrote:

From: Gopalakrishnan G <gopal2408@gmail.com>
Subject: [MW:15010] Stress relieving cycle for 6 mm welded plate
To: materials-welding@googlegroups.com
Date: Thursday, August 2, 2012, 5:34 PM

What will be the Stress relieving Cycle for 6 mm welded Plate ( IS 2062 Gr.B) as per ASME Sec VIII.what will be the rate of heating and cooling for this material? Please Help me in this regard.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...