Dears:
Normaly In Crosscountry Pipeline construction we can use Vertical Up
or Vertical Down
If Available Vertical Down is more speed than Vertical Up As tow
Posistions are accepted
Regards
Eng Mustafa Alzeer
Expirt in Crosscountry Pipeline construction &Designing
2012/7/30, BHARAT GOLE <bharatgole@hotmail.com>:
>
> In Crosscountry Pipeline construction what is welding position of Pipe on
> hill with respect to Welding Procedure as well as Welder qualification.
> Slope of hill is around 30 °.
> I had always doubt whether it is 5G or 6G ? In fact I heard always debate
> on this issue.
> Appreciate your expert comments soon.Regards
>
>
> Bharat B. Gole
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34920] Tubesheet Hole step
Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP -- https://materials-...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment