Dear sir

u can use that welder in 3/4" because As per Section-ix QW-451.4 all groove qualified welder also qualified in All fillet weld size


Regards
Jatin Dave


From: veera raghava kommisetti <kommisetti@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, 14 July 2012 9:58 AM
Subject: Re: [MW:14864] Socolet and Weldolet welding

if it is fillet weld, you can go ahead.
mostly socoletand weldolet joints are not but weld joints.

On Thu, Jul 12, 2012 at 2:27 PM, Biplab Pal <biplab.mech@googlemail.com> wrote:
Dear Expert,

I have some confusion.
My Welder is qualified with min 1 inch OD groove weld.
Can i use him in 3/4 inch NPS socolet and weldolet connection of class 3000 and 6000.
Reply with explanation and references of code.

Note: Please go through Socolet and Weldolet dimensions through chart.

--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project

E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...