Tuesday, July 3, 2012

Re: [MW:14756] Permissible value in decreasing of liquid level in hydrostatic test for aboveground storage tanks

Mr Gendia

1-Fixed roof tank
2-Open Manhole has on the roof
3-Seaside near port . its around 30-35 dgree celcious nowadays
4-No
5-No
6-Before test measured after test no

whats your comment only with this parameteres. suppose some settlement occured due to weight

2012/7/3 eccospi <eccospi@gmail.com>

Dear Mr. OZDEMIR

 

To answer your query there is some further data required:

 

1.       The tank top: Open top  or Fixed Roof or Floating Roof.

2.       Roof Venting System.

3.       The Atmospheric Temp in this specific area.

4.       Any Settlement measure being carried over while Hydrostatic testing for the Bottom??? [ by measure or visually]

5.       Shell Condition with regard to Peaking and Banding from outside [ any changes occurred] [ by measure or visually]

6.       Shell Plumpness. [ by measure or visually]

Any way as the difference in these two  measures  is 23 mm= 0.2% for the duration  5 days and if you are in Hot weather condition @ Ambient reach +29C or higher  with open top tanks or good venting system with fixed roofs you can reach such evaporation in the contained water is considered from my point of view reasonable as You need to calculate the evaporation rates to get the actual amount of loss.

 

N.B.: The level of water in Hydrostatic testing results in consideration the following:

1.            Any detected leak.[ reference duration to be done in 1 to 3 Hours]

2.            Any Deformations to the Shell or Roof.[ days as for base settlement ]

3.            Measure the Foundation Settlement while actual full loading case.

 

I hope this will be of any help to your question.

 

Best rgrds

D.eng.A.Aziz Gendia

ecco-spi President & CEO

Mob.: +2012 21 33 956

Fax: +202 2477 8411

e-mail: ecco-spi@gmail.com

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ESMAT S
Sent: Tuesday, July 03, 2012 12:49 PM
To: materials-welding@googlegroups.com
Cc: materials-welding@googlegroups.com
Subject: Re: [MW:14748] Permissible value in decreasing of liquid level in hydrostatic test for aboveground storage tanks

 

Is tank exposed to the sun?!!

Sent from my iPhone


On Jul 3, 2012, at 11:51 AM, "tugrulhan özdemir" <tugrulhan9@gmail.com> wrote:

Hi everyone

 

 

Is there anyone have an idea about  Permissible value in decreasing of liquid level  in hydrostatic test for aboveground storage tanks.

 

For example  just after filling the tank liquid level was 10610 mm   at 29degre celcious

                           after 5 days the tank liquid level was 10597 mm at 29degre celcious

 

otther infos: New tank , first time for hydrostatic test,  A36 material

 

Thank you

 

 

 

Tugrulhan OZDEMIR

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

Tuğrulhan ÖZDEMİR

Metalürji & Malzeme Müh. (Y.T.U.)

U.Kaynak Mühendisi (I.W.E.)


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...