Skip to main content

Re: [MW:13781] Clarification of PQR/WPS in FCAW process

Dear Members
 
Is any body have qualfied WPS and PQR for reference purpose only for FCAW as per AWS D1.1 for the thickeness of material from 25 mm to 50mm.
 
If the WPS is qualifed for CJP ( Complete Joint Penetraion)  is it going to qualify for for PJP ( Partial joint penetraion )  and Filler welds also.
 
Regards
 
Chinnappa Rao Basuthakr

On Mon, Jul 18, 2011 at 1:49 AM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
if nothing is mentioned for gas, it is understood that it is usable in full CO2 /Ar+co mixture


On Wed, Jul 13, 2011 at 7:12 PM, arvinda shan <arvindashan@gmail.com> wrote:
Dear Experts,
 
I need some clarification in document review. PQR qualified in FCAW process for 27 mm plate in 3G position. WPS is prepared for structural joint for 34 mm in all positions.What is the essential one?
 
  1. In FCAW proces PQR , Electrode AWS no. E71-T-1C is used. But in WPS E71-T-1 is mentioned. Whether its ok?
  2. PQR in FCAW qualifies 3G position of 27mm plates as per ASME SEc.IX and API-650. What is qualification of position in WPS for 3G whether its ALL POSITION or only 3G postion?
  3. The WPS is to be used for structural activies. ie. as per AWS D1.1. But in WPS also mentioned reference code as ASME sec.IX and AWS D1.1.
Plz clarify.
 
Thanks
 
Arvinda.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanking you

With best regards
 Rao

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...