Skip to main content

Re: [MW:13795] BASE METAL THK. RANGE AS PER ASME SEC. IX.

Dear C.R.Gandhi,

For
1) 2.95 mm. for TIG and 6.6 mm. for SMAW. and All Size for Fillets.

2) i am not sure but as per my understand QW-202.4 is for Dissimilar Base metal Thickness But, you have PQR for 6 mm(there is no dissimilar thickness).

Regards,
Chirag Patel.
Welding Engineer.
The Anup Engg. LTD.


On Tue, Feb 28, 2012 at 5:39 PM, CHINTUKUMAR GANDHI <cgandhi1975@yahoo.com> wrote:
Dear Experts,
 
Good day to all. I have 2 cases which are to be shared with you for my knowledge.
 
(1) I have qualified a WPS of 8.5 mm. Base metal Thk. of P-1 G-1 to G-2. Root Run TIG and subsequent SMAW. TIG weld deposit thk. 2.5 mm. and SMAW weld deposit thk. 6 mm. PWHT- Normalizing and Tempering with Impact test at MDMT (-45º C.)
 
As per my opinion, as per QW-403.6- Minm. T qualified shall be 1.5 mm. & Max. will be 9.35 mm. as per QW-407.4. As per QW 451.1 qualified deposited weld metal thk. range will be 2t (viz. 5 mm. for TIG and 12 mm. for SMAW.) for groove welding. and for Fillet- deposited weld metal thk. range will be all fillet size. Am I correct?
 
(2) I shall have to qualify a WPS of 6 mm. Base metal Thk. (T) of P No. 8 Group 1 to itself. Complete TIG. 
 
As per my opinion, QW-202.4 (b) (1) and QW-451.1 Min Qualified T shall be 1.5 mm. and no limitation on Max. T qualified. As per QW 451.1 qualified deposited weld metal thk. range will be max. unlimited for groove welding. and for Fillet- deposited weld metal thk. range will be all fillet size. Am I correct?
 
Please share your experience with me on urgent basis.
 
Thanks & regards,
 
C. R. GANDHI
(Manager- Q. C.)
 
  
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...