Skip to main content

[MW:13726] dished head shape for 2: 1 elleptical dished head

Dear All,
 
Greetings.
 
A dished head of  ID 1520 mm & thk 80 mm hot formed by subcotractor. A vessel is being manufactured by ASME SEC VIII DIV1.
as per the forming report  dished head is having Overcrowning of 10 mm & SF is 70 mm.
 
 Now vessel manufacturer  is claming that Dished is having 10 mm plus side SF( 80 mm). manufacturer wants to shift tan line by 10 mm to maintain overall lenght.
 
my question is --
 
1)  is it mandatory that for  for a dished having overcrowing,  SF  will also be more than required.
 
2) what is the effect on Knuckle radius if the SF is shifted by 10mm.( considering the fact that contractor  has  done forming of the dished head considering 70 mm SF).
 
3) can we accept the dished head if  dished head forming contactor certify that even with 80MM SF the true shape of  the dished head will be satisfactory.
 
can we accept the dished head if  true shape of the  dished head  is checked by a template( 2: 1 elleptical type) which is having 80mm SF & it is showing satisfactory result.
 
Please advice.
 
Thanks & Regards
 
Asad Azmi
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...