Skip to main content

RE: [MW:13766] RE: 13746] TURBALOY® 17-22 (US WELDING)

No. 

 

This alloy is closer to AISI 4140 or 4130.  The addition of V and higher Carbon permit higher strength with adequate ductility.  The web page cited below lists several of the materials where this electrode is used.  You will find that these materials are used in steam turbines, turbine shafts, and where a high strength, heat treatable, alloy steel is required.  Standard B2 chemistry will not achieve the same properties as the turballoy or the base material.  I would expect that a closer substitution would be filler metals intended for use in welding 4140 but you would have to investigate this for yourself. 

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Roy LIU??
Sent: Monday, February 20, 2012 10:50 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:13757] RE: 13746] TURBALOY® 17-22 (US WELDING)

 


Thank you John.
This material is rarely found in China, So I am confused.

As per the chemical contents, this material is fimilar with E80S-B2 (AWS), but carbon contents and
 nd copper coated types are different.
I supposed that this material is designed only for military. But they are nearly the same!

I read the description, this
 GMAW wire is suitable for 1.25 % Cr 0.5 % Mo alloyed boiler, plate and tube steels as well as for the welding of Q&T steels.  

Can ER80S-B2 take the place of
 TURBALOY 17-22?

Any of your help will be appreciated!

 

  Best regards

 

  Roy 

 


Subject: [MW:13756] RE: 13746] TURBALOY® 17-22 (US WELDING)
Date: Mon, 20 Feb 2012 09:12:37 -0600
From: jhenning@deltak.com
To: materials-welding@googlegroups.com

This is a specialty filler metal, 1¼Cr-½Mo base with the addition of vanadium and high carbon content (relative to most filler metals).  This material does not conform to any AWS/ASME  classification.  Typical applications are listed in the US Welding Corp. literature.  See:   http://www.usweldingcorp.com/TDS/tds6458.pdf

 

It is used for welding and repair of similar materials in turbines etc.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Roy LIU??
Sent: Monday, February 20, 2012 12:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:13746] TURBALOY® 17-22 (US WELDING)

 

Hi, Experts,
Could anyone teach me what the
 TURBALOY® 17-22 material is?
I can not find the proper AWS code for this material.

this datasheet shows us nothing! (below link)
http://usweldingcorp.com/MSDS/6458.pdf

Thanks!!

 

Best regards

 

Roy 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...