[MW:13692] RE: Drop Weight Test.

Hi Mohit,
 
The purpose of drop weight test is to detect the Nil Ductility Temperature (NDT).The applicable standard is ASTM E-208. See the attached brief description for your information.Sec-III, NB2330 explains the basis for establishing the NDT.
 
Hope this would clarify your query.
 
Thanks.
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist & Consultant

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: Mohit Aggarwal [mailto:aggarwalmohit05@gmail.com]
Sent: Tuesday, February 14, 2012 10:17 AM
To: materials-welding
Cc: christopher_rajku...@yahoo.com; george.dilintas@gr.bureauveritas.com; manojac...@gmail.com; welding_engr_r...@charter.net; AA karandish; Abuhanip bin Abdul; Ahmed Osman; akcme; Ali Asghari; Aly; AMIT PAHUJA; Amos Majola; Anil Hegde; antony jenis; Arun Jacob; Arunachalam A; Ary Agung Prasetyo; asad azmi; Brl Pp; Dindo; Dinesh Somwanshi; duc hoang; ENAYAT ZAREI; Endri Prasetyo; Fitria Rahman; fredric; Garry Mat Eng.; Himan Nikdin; james gerald; John Henning; jose; Kaja Mohideen; kannayeram gnanapandithan; Karthik; Kavin Murugam; ketan shah; khemici badri; lakshman kumar; Madhusudan Rout; mahesh sanghvi; Mahmoud; meemo prasad; Mehdi Emami; mpk mpk; MRG; Muhammed Ibrahim PK; muthu barathi; Nadgauda, Subhas; Nandesh Kumar; Narendra Gohil; Neilash Kumar; Nizam Mohamad; pgoswami; Pieper QSI; prabhakarmet@gmail.com; prem nautiyal; R.Lenin; rajeev arora; rajkumarantoni; Ramchandra vichare; Ramin Kondori; ravi varman; S C Balawat; sanggyu LEE; santhosh kumar; SAQIB SHIRAZI; sevak hiren; Shadab Alam Ansari; shanmuga mari; snbagchi; Srinivas Engr; srinivasu; T. Mahendran; U WYNN-NAING; vaibhav Joshi; venkat ramana; Vijay Katkar; vinit.deshpande; Vino Varghese; Wu Hua; yogeshkumar Kumbhar; ZUL MAS
Subject: Drop Weight Test.

Respected Experts,

As per client Requirement We will have to conduct Drop  Weight Test IN NPCIL.. What is Drop Weight Test and how we will determine Nil ductility transition temp..PLease reply

Thanks & REgards
MOhit Aggarwal.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...