Saturday, September 3, 2011

Re: [MW:12438] Query / Machining of Sch 40 to Sch 30 / 24 RF WN Flange

Dear,
You can use a fitting of Sch-40 and machined its edge to match
the thickness of sch-30 . Vineet
Sent using a Sony Ericsson mobile phone


---- Original message ----
From:
Sent:
To:
Subject: Re: [MW:12321] Query / Machining of Sch 40 to Sch 30 / 24 RF WN Flange

Is it mean trimmed/chamfered? Code is allowed, you can see the sizes/figure in the B16.5 book, but certain customers require ID of flange same with ID of pipe.


Sent from my Hape Buluk®
powered by Sinyal Lieur INDOSAT

-----Original Message-----
From: Vino Varghese <vinopvarghese@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Sat, 27 Aug 2011 15:04:12
To: <materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:12316] Query / Machining of Sch 40 to Sch 30 / 24" RF WN Flange

Dear All,

I would like to know whether standard *ASME B 16.5* do allow machining of
bevel edge to achieve required thickness?
*The material is 24" WN RF Flange A105 ,Class 150- NACE , Normalised*.

We are not able to procure standard fitting and done machining to achieve
Sch 30 from Sch 40. Please note, *not to entire length*.
The dimension and thickness is verified and a Certificate of Compliance is
produced.

Please advise with evidence(supporting Code) whether the material could be
ACCEPTABLE.

*Thanks & Regards*
*Vino-Doha*

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...