Wednesday, September 7, 2011

Re: [MW:12362] WPS based on contractor PQR

generally if your client is agreed with your documnets with no objection you can use his wps & pqr under the supervision of same client.

regards

dinesh

On Wed, Sep 7, 2011 at 3:01 PM, G Padmanabhan <gpadmana@gmail.com> wrote:
Hi,
As per ASME Sec IX,  EPC Contractor qualified WPS/PQR for carbon steel material.Based on contractor qualified PQR,whether subcontractor can prepare WPS and use for welding. EPC contractor will take operational control and responsibility of welding activities.

 code of construction is ASME B31.3.

Please throw some light on QW 200.


--
Nothing is difficult, you just didn´t understand it yet...
 
With Warm regards,

G.Padmanabhan


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...