Wednesday, September 7, 2011

[MW:12354] SMAW ELECTRODE FOR P91 MATERIAL

Dear Group Members,

I am having 3 approved WPSs for P91 material.These 3 WPS are using 3
different electrodes.

1)9018-B9 -Iron powder & Low hydrogen potassium coated
2)9016-B9 -Low hydrogen potassium flux coated
3)9015-B9 - Low hydrogen sodium flux coated

My doubts are

1)How we can justify which electrode is better for my use?
2)Any where in code it mentioned the suitable flux coating for
electrode?


Regards

Jose Sebastian
+919687660525

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...