Dear Kundan/Mayur,

ASME Section IX Welder Qualification related Question.

As mentioned in section IX for qualification of welder or welding
operator use qualified WPS with supporting PQR's, if our PQR is welded
with P No- 8 to P No-8 (SA 240 TP 316L TO SA 240 TP 316L).

Is it possible to make WPS with P No-1 to P no-1 (PQR is with P No -8
To P No-8) but other than p no all variable are same as used in PQR
(Like filler wire, shelding gas, purging if require or etc), this WPS
will use only for welder qualification. please guide us.

Vijay Katkar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35536] RANGE ASME SEC IX

Dear All we have qualified WPS for ( ASME SEC IX) 1. BASE plate 8 mm ( 8TO 16 mm RANGE WITH IMPACT )  2 . BASE plate 25 mm ( 16TO 50mm RANGE...