RE: [MW:9474] EN 287-1 Interpretation

Hi,
As per 5.4 and in your case,You need to qualify the welders for fillet welding.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 1/25/11, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:

From: Elshan Feyzullayev <elshan_f@hotmail.com>
Subject: RE: [MW:9454] EN 287-1 Interpretation
To: materials-welding@googlegroups.com
Date: Tuesday, January 25, 2011, 7:06 PM

Dear Limesh,

I don't have EN 287-1 in hands. But as per AWS D1.1 qualification of CJP groove welds qualifies for fillet welds.
But my undestanding from below highlighted extraction from EN 287-1 taking into account that the majority of your welds are fillet so you should qualify your welders by an appropriate fillet weld test.

best regards,
Elshan.


Date: Tue, 25 Jan 2011 15:15:21 +0400
Subject: [MW:9449] EN 287-1 Interpretation
From: limesh78@gmail.com
To: materials-welding@googlegroups.com

Dear All,

 

Welder Qualification Code - EN 287-1,2004 Edition.

I have to fabricate some pipe supports and most of the work comes under fillet weld. I have some qualified welders as per EN 287-1 in plate 'butt weld' for all position. Are they qualified to weld these fillet welds as majority of the work comes under fillet weld? Should I requalify my welders in plate 'fillet weld' to fabricate these supports? I am looking for the correct interpretation of the following clause which is highlighted in yellow colour.

 

As per EN 287-1 ,2004 edition,5.4 Type of weld
 

b) in cases where the majority of work is fillet welding, the welder shall also be qualified by an appropriate fillet

welding test; in cases where the majority of work is butt welding, butt welds qualify fillet welds;
 
Regards,
Limesh
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...