Dear Moin!
                   Please see ASME 31.3 Chapter III  (Materials and specification) 323.1, 323.2, etc., has listed, Listed and unlisted materials.  Normally  A 36 will not meets A234 chemical, mechanical properties,If your project specification included A 36 material for fittings then you can use other wise you cannot use that SA 36 instead of SA 234

On Tue, Jan 25, 2011 at 5:46 PM, Moin - QC <Syed.Moin@gerabgroup.com> wrote:

Dear Krishnasamy,

 

Thanks for the information but is there any restriction in code B31.3 or BPV

 

REGARDS,
SYED MOIN

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of KRISHNASAMY MASANAM
Sent: Tuesday, January 25, 2011 2:50 PM

Subject: RE: [MW:9447] ASTM A36 plates

 

Dear Moin!
                      A36is carbon steel for general structural purposes and also A234 is wroyght carbon steel with Chromium (for forming stable matel carbides at the grain boundaries and the strong increase in corrosion resistances). Molybdenum (used in steels alloys for its high corrosion resistace and weldablity), Nickel (for instance, the austenite structure of iron is stabilized. This crystal structure makes such steels  less brittle at low temperatures) etc., these items are missing in A36. So your client statement is correct...        

Thanks & Best regards

 

Krishnasamy. M

Welding Inspector

Fize Al- Shammary Gen. Cont. Est.

Kingdom of Saudi Arabia.

Mob: +966 592823768




 


Date: Tue, 25 Jan 2011 02:14:55 +0000
To: materials-welding@googlegroups.com
Subject: Re: [MW:9443] ASTM A36 plates
From: manpreetsin88@rediffmail.com

Dear Moin,

Yes, your client is correct, A36  is a commonly known as structural plate with poor grain structure and should not be used for pressure vessels,

Why not try SA516, there is not much cost difference.


Regards
Manpreet Singh





On Mon, 24 Jan 2011 19:11:41 +0530 "Moin - QC" wrote
>

Dear members,

Can a plate to ASTM A36 can be used to manufacture TEEs to A234 WPB, is there any restriction in BPV or B31.3 on the use of A36 plate for manufacturing A234 Tees.

One of client says A36 is for general purpose and cannot be used for making a pressure containing component to be used in oil and gas production . Is it correct, if yes why? And if not can you please provide me a technical justification, I could not find anything B31.3.

Thanks & Regards
>
Syed Moin
>


>______________________________________________________
>CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
>________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please visit http://www.messagelabs.com/email
>______________________________________________________________________
>
--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
Image removed by sender.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...