Re: [MW:9455] sfa specification for ER 316L

SFA 5.28 is for Low Alloys Steel
SFA 5.9   is for Stainless Steel
   It may be editorial mistake and it is not a essential variable, u can correct and sign
Pandithan

On Sun, Jan 23, 2011 at 4:44 PM, VENKATA SWAMI REDDY KARRI <kvsreddy777@gmail.com> wrote:
Dear all,
 
 
previews project wps showing SFA NO AWS 5.28 for ER 316L But it is approved by client and PQR also stated that same as WPS. actually it is 5.9 as of my knowledge. Does anybody know any special thing there about 5.28 for ER316L

--
 

Best Regards,

K.V.S.Reddy,
Q.C.Inspector(Piping&Welding),
BS-132 Project,
SKEC Eng& Con Ltd.,
Postbox no-55653,
Sabahiya-54567,
Kuwait.
kvsreddy777@gmail.com,karryswamireddy@yahoo.com,
Ph:00965-94414396.
PleaseSave a tree. Don't print this e-mail unless it's really necessary
L

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...