Tuesday, January 25, 2011

RE: [MW:9454] EN 287-1 Interpretation

Dear Limesh,

I don't have EN 287-1 in hands. But as per AWS D1.1 qualification of CJP groove welds qualifies for fillet welds.
But my undestanding from below highlighted extraction from EN 287-1 taking into account that the majority of your welds are fillet so you should qualify your welders by an appropriate fillet weld test.

best regards,
Elshan.


Date: Tue, 25 Jan 2011 15:15:21 +0400
Subject: [MW:9449] EN 287-1 Interpretation
From: limesh78@gmail.com
To: materials-welding@googlegroups.com

Dear All,

 

Welder Qualification Code - EN 287-1,2004 Edition.

I have to fabricate some pipe supports and most of the work comes under fillet weld. I have some qualified welders as per EN 287-1 in plate 'butt weld' for all position. Are they qualified to weld these fillet welds as majority of the work comes under fillet weld? Should I requalify my welders in plate 'fillet weld' to fabricate these supports? I am looking for the correct interpretation of the following clause which is highlighted in yellow colour.

 

As per EN 287-1 ,2004 edition,5.4 Type of weld
 

b) in cases where the majority of work is fillet welding, the welder shall also be qualified by an appropriate fillet

welding test; in cases where the majority of work is butt welding, butt welds qualify fillet welds;
 
Regards,
Limesh
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...