When the assembly is being PWHT’ed, EM14K may be selected to maintain properties.  This is especially the case where some of the assembly is either P4 or P5A and for which separate PWHT is not practical.  In such a case, EM14K is a better choice than EM12K.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of muthusrinivasan muthuselvam
Sent: Tuesday, January 25, 2011 3:16 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9447] SAW filler for SA516 Gr70

 

F7A4 - EM12K it self sufficient. No need to go for High magnese EM 14K..

 


BR,

MSMS

On Sat, Jan 15, 2011 at 12:14 AM, rinshad abdul rahman <rinshad043@gmail.com> wrote:

Dear all,

 

Which is the suitable filler for SAW on SA 516 Gr70 (with PWHT) ?

 

EM12K or EM14K

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...