Tuesday, January 18, 2011

Re: [MW:9305] Wash Pass

thanks ajay..... btw my client was catch welder wash pass at buttering..... he argue coz in wps not stated for this tecnique..... all of buttering had finished was remove for reweld coz of this..... could u or anybody know if has any standard for this technique for auto gtaw?



On Mon, Jan 17, 2011 at 10:27 PM, ajay pawse <ajaypavashe@yahoo.com> wrote:
Hi,
 
Wash pass is a just fusion pass without addition of filler material. i t is recommended over at least one pass with filler (625 overlay etc)
 
Regards,
Ajay

--- On Mon, 17/1/11, fariza a rahman <fariza.arahman@gmail.com> wrote:

From: fariza a rahman <fariza.arahman@gmail.com>
Subject: [MW:9247] Wash Pass
To: materials-welding@googlegroups.com
Date: Monday, 17 January, 2011, 12:46 AM

Hi all...

Anybody know about wash pass.What material can use this technique and what effect of this.Can use for cladding(Inc 625),buttering(13.40) to base material F22?

TQ.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...