Dear Akhil,
You can recertify the material if it conforms to your new edition of construction, Provided
1. If the material is also certified to equivalent ASTM standard and the edition is in the range specified in the Guidelines on acceptable ASTM editions in Sec.IIA (In front from page no.xix) . or within bracket information below the specification headline of the material.
2. If you can prepare a comparison chart to prove both earlier edition and new edition are identical for the particular material by all means.
Thanks and regards,
K.Rajagopal

On Tue, Jan 18, 2011 at 2:58 PM, Akhil Chemmarathil <akhilcme@gmail.com> wrote:
Dear Mr. Rajgopal,

I am going to do the vessel as per ASME 2007Ed and 2009 Add. But my TDC and PO is for the same, the certificate received for the plate material is as per 2004 Ed and 2006 Add and the date of manufacture of the plate is 15.05.2008. i.e, at the time of manufacture 2007 edition was valid still they certified as per 2004 Edition.


Will it be a problem evenif the material confirms to 2007 Ed and 2009 Add???


Regards

Akhil

On Tue, Jan 18, 2011 at 2:02 PM, Rajagopal Kannan <rajagopal.kannan@gmail.com> wrote:
Dear akhil,
2007 edition is valid from Jan 2008. But if you have mentioned in the contract with client before 2008 about certifying the vessel according to 2004 edition 2006 addenda, you can manufacture it to that addenda at any time.
This is my understanding.
Thanks and Best Regards,
K.Rajagopal

On Tue, Jan 18, 2011 at 1:54 PM, akcme <akhilcme@gmail.com> wrote:
Dear All,

I have received a material test certificate confirming to ASME BPV
Code 2004 Edition 2006 Addenda. But the manufacturing date is
15.05.2008.

Please let me know about, From which date onwards ASME BPV Code 2007
was valid.

Please advice

Regards

Akhil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...