that its not a fillet weld
Sadique Sheikh <sadiq.mech@gmail.com>Sent by: materials-welding@googlegroups.com01/03/2011 06:20 PM
Please respond to
materials-welding@googlegroups.com
Tomaterials-welding@googlegroups.com cc SubjectRe: [MW:9063] UT of Fillet weld
Actually I want to know the defect of incomplete fusion in T-joint
fillet weld.Please see attached Drawing for reference. In that Can we
know about fusion on plate A with welding with angle probe or we must
need TR probe to identify the defect? Bevel angle side fusion we get
with angle probe.
On Mon, Jan 3, 2011 at 2:51 PM, muthusrinivasan muthuselvam
<msms2k@gmail.com> wrote:
> Dear Mr.Sadique..
>
> what you are looking exactly in fillet weld UT..
>
> Can you elaborate little bit..
>
> br,
> msms
>
> On Mon, Jan 3, 2011 at 1:40 PM, Sadique Sheikh <sadiq.mech@gmail.com> wrote:
>>
>> Dear All,
>> During UT inspection of fillet weld, Does we need both angle probe and
>> normal or TR probe?
>>
>> Thanks & Regards,
>> Mohd. Sadique Sheikh
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/--
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
To post to this group, send email to materials-welding@googlegroups.comhttp://materials-welding.blogspot.com/
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
This electronic mail content and any accompanying attachments ("the Message") is intended only for the named addressee ("the Recipient") and may contain information that is confidential, privileged and/or proprietary to the Sime Darby group of companies ("Sime Darby") and/or protected under applicable laws. If you are not the intended Recipient, you are strictly prohibited from using, disseminating, forwarding and/or printing the Message. Please notify the sender immediately by return e-mail and permanently delete all copies of the Message. Sime Darby disclaims all liability for any error, loss or damage arising from the Message being infected by computer virus or other malicious software. Any views and/or opinions expressed in the Message are solely those of the author's and do not necessarily represent those of Sime Darby's.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment