Dear All,

Can somebody advice me about the use of A234 WPB fittings in the
place of A420 Gr.WPL6 for the LPG line.

I hope,A234 WPB is for medium and elevated temperatures,whereas A420
is for lower operating temperatures. and moreover A420 is having
impact test properties.

So i hope we cant use the A234 WPB in place of A420,even though
tensile properties are same.

In my project,Design Temperature of LPG line is -45 deg to +85 deg.

Is my statement is correct?


Regards,


Thiru.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...