Dear All,
 
Can you help me out with a Material Comparison Chart for S275 JR against API 5L X 52.
I am mainly looking for Physical and Chemical Properties.
 
This is required for WPS Qualification for S275 JR Material as per Project Requirement. 
The PQR is qualified with X52 Material.
 
The Change of Material Grade/Type is essential Variable in Project Specification.
The Comparison Chart can provide a source to convience Client.
 
Hope to see a positive response from Experts.
 
Thanks & Regards
Vino P Varghese
Doha-Qatar
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...